Effect of Magnesium Treatment on Inclusion Formation and Solidification Structure Ferrite Stainless Steel 430
Special SteelVol. 34, Issue 2, Pages: 48-51(2013)
作者机构:
1. 上海交通大学金属基复合材料国家重点实验室,上海,200240
2. 宝山钢铁股份有限公司研究院,上海,201900
作者简介:
基金信息:
DOI:
CLC:
Received:10 October 2012,
Online First:08 October 2022,
Published:08 October 2013
稿件说明:
移动端阅览
公茂涛, 陈兆平, 徐迎铁, et al. Effect of Magnesium Treatment on Inclusion Formation and Solidification Structure Ferrite Stainless Steel 430[J]. Special Steel, 2013, 34(2): 48-51.
DOI:
公茂涛, 陈兆平, 徐迎铁, et al. Effect of Magnesium Treatment on Inclusion Formation and Solidification Structure Ferrite Stainless Steel 430[J]. Special Steel, 2013, 34(2): 48-51.DOI:
Effect of Magnesium Treatment on Inclusion Formation and Solidification Structure Ferrite Stainless Steel 430
The effect of 0. 000 5% ~Q. 001 2% Mg on inclusion formation and solidification structure of ferrite stainless steel 430 (/% : 0.04C
0.25-0.32Si
0.28-0.38Mn
16.5-16.9Cr) melting by a 60 kg vacuum induction furnace has been tested and studied. Results show that with adding magnesium alloy in liquid steel 430 the size of MgO compound inclusions in steel decreases while their number and density are increase; adding magnesium alloy is available io improve the solidification structure of steel 430 and the lower the casting temperature the more obvious the improved effect
for instance with casting at 1 580 ℃ the equiaxed zone ratio of magnesium-treated steel increases to 88.5% from 30.8% of non-treated normal steel while the correspondent equiaxed grain size decreases to 945.3 μm from 1741.6 μm. The planar dis-registry between inclusions containing MgO and δ phase is minor
it is an effective heterogeneous nucleation agent to promote the formation of equiaxed crystal and inhibit the growth of columnar crystal
finally fine the solidification structure of casting steel 430.