您当前的位置:
首页 >
文章列表页 >
Cleanliness of Low Carbon Al-Killed Steel Produced by 200 t LD-LBAr-CC Flow Sheet
更新时间:2026-01-21
    • Cleanliness of Low Carbon Al-Killed Steel Produced by 200 t LD-LBAr-CC Flow Sheet

    • Special Steel   Vol. 34, Issue 2, Pages: 45-47(2013)
    • Received:22 October 2012,

      Online First:08 October 2022,

      Published:08 October 2013

    移动端阅览

  • 易正明, 肖慧. Cleanliness of Low Carbon Al-Killed Steel Produced by 200 t LD-LBAr-CC Flow Sheet[J]. Special Steel, 2013, 34(2): 45-47. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Metal Pretreatment-80 t LD-RH-LF-CC Process Flow on Inclusion in Pipeline Steel
Examination and Study on Cleanliness of Non-Oriented Silicon Steel XG800WR in 210 t BOF-RH-CC Steelmaking Process
Effect of Different Residual Steel Amounts on Molten Steel Cleanliness
Effect of Refining Slag Basicity on the Molten Steel Cleanliness of GCr15SiMn Bearing Steel
Development of Continuous Casting Round Billet for P92 Heat-resistant Steel for Ultra-supercritical Boiler Tubes

Related Author

王国承
黄浪
吴绍杰
万勇
陈伟庆
于彦冲
Ren Ying
Liu Zhonghua

Related Institution

江西理工大学材料与化学工程学院
新余钢铁公司
北京科技大学冶金与生态工程学院
新余钢铁公司技术中心
School of Mechanical and Materials Engineering, North China University of Technology
0