Numerical Simulation of Effect of Casting Speed on Level Fluctuation of Liquid in Billet Mold
|更新时间:2026-01-21
|
Numerical Simulation of Effect of Casting Speed on Level Fluctuation of Liquid in Billet Mold
Special SteelVol. 34, Issue 6, Pages: 14-17(2013)
作者机构:
北京科技大学冶金与生态工程学院,北京,100083
作者简介:
基金信息:
DOI:
CLC:
Received:24 June 2013,
Online First:06 September 2022,
Published:06 September 2013
稿件说明:
移动端阅览
韩毅彤, 张炯明, 罗衍昭, et al. Numerical Simulation of Effect of Casting Speed on Level Fluctuation of Liquid in Billet Mold[J]. Special Steel, 2013, 34(6): 14-17.
DOI:
韩毅彤, 张炯明, 罗衍昭, et al. Numerical Simulation of Effect of Casting Speed on Level Fluctuation of Liquid in Billet Mold[J]. Special Steel, 2013, 34(6): 14-17.DOI:
Numerical Simulation of Effect of Casting Speed on Level Fluctuation of Liquid in Billet Mold
With using established "liquid-slag" two phase flow model in mold for 180 mm x 180 mm billet by fluid mechanics software Fluent
the numerical simulation on behavior of liquid level fluctuation is carried out to study the effect of deviation distance of submerged nozzle from mold center (0 ~ 30 mm) and casting speed (2. 0 ~3. 0 m/min) on behavior of level fluctuation of liquid in mold. It is found that at same deviation distance of submerged nozzle
with increasing the casting speed
the trend of the whole for liquid level fluctuation increases
and the more of deviation distance and casting speed
the more of increment of liquid level fluctuation ; at low casting speed
the wave troughs occur at edge of nozzle with violent fluctuations around nozzle outlet; at high casting speed
the wave troughs occur at right wall of mold to intensify the liquid level fluctuation and easily form slag entrapment.