Process Flow Sheet and Internal Quality Control of Domestic 1215 Low Carbon High Sulphur Free-Cutting Steel
|更新时间:2026-01-21
|
Process Flow Sheet and Internal Quality Control of Domestic 1215 Low Carbon High Sulphur Free-Cutting Steel
Special SteelVol. 34, Issue 4, Pages: 29-32(2013)
作者机构:
北京科技大学冶金与生态工程学院,北京,100083
作者简介:
基金信息:
DOI:
CLC:
Received:20 February 2013,
Online First:11 September 2022,
Published:11 September 2013
稿件说明:
移动端阅览
林腾昌, 朱荣, 王成杰, et al. Process Flow Sheet and Internal Quality Control of Domestic 1215 Low Carbon High Sulphur Free-Cutting Steel[J]. Special Steel, 2013, 34(4): 29-32.
DOI:
林腾昌, 朱荣, 王成杰, et al. Process Flow Sheet and Internal Quality Control of Domestic 1215 Low Carbon High Sulphur Free-Cutting Steel[J]. Special Steel, 2013, 34(4): 29-32.DOI:
Process Flow Sheet and Internal Quality Control of Domestic 1215 Low Carbon High Sulphur Free-Cutting Steel
An analysis on the products of 1215 low carbon high Sulphur free-cutting steel (/%: 0. 05 ~ 0. 10C
W 0.013Si
1.06 ~1.33Mn
0. 051 -0.061P
0. 24 ~0. 36S
0.012 0 ~0. 014 0[O]
0.005Al) produced by domestic 100 t EAF-LF-CC
80 t
100 t and 160 t BOF-LF-CC four process production line is carried out. Results show that the control characteristic of domestic 1215 low carbon high Sulphur free-cutting steel is to control Mn/S (3. 7 - 3. 9) of steel by suitable increasing Mn content in steel and for individual flow sheet is by decreasing S content in steel to get Mn/S =4. 4; the inclusion control of inclusion in steel produced by 160 t BOF flow sheet (Mn/S =3. 8
fluctuation of MnS inclusions area and length/width ratio are comparatively smaller) is better than that by others; due to smaller segregation of elements in casting billet and suitable controlling of cooling rate after rolling the steel produced by 80 t BOF flow sheet and 160 t flow sheet has no obvious banded structure
but by 100 t EAF flow sheet and 100 t BOF flow sheet the rating of banded structure is 3 ~4.