Finite Element Simulation of Hot Continuous Rolling Process of Gear Steel 20CrMnTi Bar Products
|更新时间:2026-01-21
|
Finite Element Simulation of Hot Continuous Rolling Process of Gear Steel 20CrMnTi Bar Products
Special SteelVol. 35, Issue 2, Pages: 16-19(2014)
作者机构:
北京科技大学材料科学与工程学院,北京,100083
作者简介:
基金信息:
DOI:
CLC:
Received:21 October 2013,
Online First:07 September 2022,
Published:07 September 2014
稿件说明:
移动端阅览
肖玉, 洪慧平, 冯富春. Finite Element Simulation of Hot Continuous Rolling Process of Gear Steel 20CrMnTi Bar Products[J]. Special Steel, 2014, 35(2): 16-19.
DOI:
肖玉, 洪慧平, 冯富春. Finite Element Simulation of Hot Continuous Rolling Process of Gear Steel 20CrMnTi Bar Products[J]. Special Steel, 2014, 35(2): 16-19.DOI:
Finite Element Simulation of Hot Continuous Rolling Process of Gear Steel 20CrMnTi Bar Products
A Hensel-Spittel flow stress model of steel 20CrMnTi with strain 0 ~0.8 and strain rate 0-3 s
-1
at 800-1150 °C is established by analysis on hot continuous rolling process of round bar. With using finite element software LARSTRAN/SHAPE the simulation of process of steel 20CrMnTi with 8 pass rolling from 200 mm x 200 mm billet to ①90 mm round bar has been carried out to analyze the variation of stress
strain and temperature field
and rolling force and torque of rolling stock during process of rolling by round pass with curved side wall and round pass with straight-line side wall. Simulated results show that at round comer of stock the equivalent stress and equivalent strain are bigger and the temperature is lower than that at other region
so the defects easily occur at the comer of stock ; the precision of round bar rolled by round pass with curved side wall is slightly hig
her that by round pass with straight-line side wall.