A Study on Model of Cutting Roll Pass Profile Spread for Hot-Rolled U-Steel Sheet Pile
更新时间:2026-01-21
    • A Study on Model of Cutting Roll Pass Profile Spread for Hot-Rolled U-Steel Sheet Pile

    • Special Steel   Vol. 35, Issue 3, Pages: 5-7(2014)
    • Received:02 December 2013,

      Online First:27 August 2022,

      Published:27 August 2014

    移动端阅览

  • 周庆鹏, 王盼盼, 杨光, et al. A Study on Model of Cutting Roll Pass Profile Spread for Hot-Rolled U-Steel Sheet Pile[J]. Special Steel, 2014, 35(3): 5-7. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Simulation Test on Effect of Rolling Lubrication and Velocity Difference on End Bending of Hot-Rolled U-Section Sheet Piling
Hot Deformation Behavior and Dynamic Recrystallization of Cold Heading Steel SWRCH22A
Finite Element Simulation on Continuous Rolling Process of Bearing Steel GCrl5

Related Author

张振兴
刘升
赵刚
魏福龙
李正嵩
杨林
程剑
叶传龙

Related Institution

武汉钢铁集团公司港务公司
首钢水城钢铁(集团)有限责任公司技术中心
北京科技大学材料科学与工程学院
0