Research and Development of Low Welding Sensitiveness Low Carbon Bainite High Strength Steel Q800CFE Plate
|更新时间:2026-01-21
|
Research and Development of Low Welding Sensitiveness Low Carbon Bainite High Strength Steel Q800CFE Plate
Special SteelVol. 35, Issue 2, Pages: 51-53(2014)
作者机构:
作者简介:
基金信息:
DOI:
CLC:
Received:17 September 2013,
Online First:14 September 2022,
Published:14 September 2014
稿件说明:
移动端阅览
刘丽华. Research and Development of Low Welding Sensitiveness Low Carbon Bainite High Strength Steel Q800CFE Plate[J]. Special Steel, 2014, 35(2): 51-53.
DOI:
刘丽华. Research and Development of Low Welding Sensitiveness Low Carbon Bainite High Strength Steel Q800CFE Plate[J]. Special Steel, 2014, 35(2): 51-53.DOI:
Research and Development of Low Welding Sensitiveness Low Carbon Bainite High Strength Steel Q800CFE Plate
研发的25 mm Q800CFE钢板(/%:0.04~0.08C,0.20~0.50Si,1.50~1.80Mn,≤0.015P,≤0.005S,0.015~0.060Nb,≤0.30Mo,≤0.03Ti,0.0008~0.0030B;裂纹敏感性指数≤0.23)的冶金流程为铁水预处理-120 t转炉-LF-RH-220 mm CC-轧制工艺。成品板终轧≤850℃,水冷至≤400℃,冷却速度20~30℃/s,并进行530~635℃回火处理。测试了Q800CFE钢板的动态连续冷却转变(CCT)曲线,研究了回火温度对组织和力学性能的影响,以及试验了该钢的焊接性能。结果表明,随回火温度增加,板条组织尺寸增大;在530℃回火时,Q800CFE钢板具有较优的力学性能,抗拉强度≥900 MPa、伸长率≥15%,-40℃夏比冲击功≥100 J;25 mm板室温下预热75℃焊接接头即可防止产生冷裂纹。
Abstract
The metallurgical flow sheet of developed 25 mm Q800CFE steel plate (/% : 0.04-0.08C
0.20-0.50Si
1.50-1.80Mn
≤0.015P
≤0.005S
0.015-0.060Nb
≤0.30Mo
≤0.03Ti
0.0008-0.0030B; crack sensitivity index ≤0.23) is metal pretreatment-120 t BOF-LF-RH-220 mm CC-rolling process. Finishing plate rolling temperature is ≤850 °C
water cooling to ≤400 ℃ with cooling rate 20-30 °C/st and tempering treatment is carried out at 530-535 The dynamic continuous cooling transformation (CCT) curves of Q800CFE steel plate is measured and the effect of tempering temperature on structure and mechanical properties and the wielding behavior of steel plate are studied. Results show that with increasing tempering temperature the size of lath structure increases; with tempering at 530 X.
the Q800CFE steel plate has optimum mechanical properties
its tensile strength ≥900 MPa
elongation ≥15%
-40 ℃ Charpy impact energy 100 J ; and the cold crack in weld joint shall be avoided as the ambient 25 mm plate is preheated to 75 °C.