Numerical Simulation of Gas-Slag-Liquid Three-Phase Flow Field in 210 t Ladle Furnace Refining Bottom Argon Blowing Process
|更新时间:2026-01-21
|
Numerical Simulation of Gas-Slag-Liquid Three-Phase Flow Field in 210 t Ladle Furnace Refining Bottom Argon Blowing Process
Special SteelVol. 35, Issue 4, Pages: 12-15(2014)
作者机构:
1. 北京矿冶研究总院,北京,100160
2. 北京华胜高技术股份有限公司,北京,100083
作者简介:
基金信息:
DOI:
CLC:
Received:08 March 2014,
Online First:02 September 2022,
Published:02 September 2014
稿件说明:
移动端阅览
储莹, 霍朝宾. Numerical Simulation of Gas-Slag-Liquid Three-Phase Flow Field in 210 t Ladle Furnace Refining Bottom Argon Blowing Process[J]. Special Steel, 2014, 35(4): 12-15.
DOI:
储莹, 霍朝宾. Numerical Simulation of Gas-Slag-Liquid Three-Phase Flow Field in 210 t Ladle Furnace Refining Bottom Argon Blowing Process[J]. Special Steel, 2014, 35(4): 12-15.DOI:
Numerical Simulation of Gas-Slag-Liquid Three-Phase Flow Field in 210 t Ladle Furnace Refining Bottom Argon Blowing Process
the numerical simulation and analysis on gas-slag-liquid three- phase flow field in 210 t ladle furnace (LF) during argon blowing have been carried out by using CFD fluid engineering simulation software FLUENT6. 3.26 to get the effect of bottom blowing porous plug position (single center plug
single eccentric plug and double plugs) and argon flow rate (100 ~500 L/min) on behavior of liquid circle flow
size of slag eye and slag entrapment. Study results show that with different bottom porous plug position the liquid mixing speed and size of slag eye are different; the slag is easily entrapped by liquid at slag eye; the stagnation zone with double plugs bottom blowing is quite small than that with single plug bottom blowing; the more argon flow rate the more dimension of slag eye
as diameter of slag eye is more than 611 mm the change of dimension of slag eye is small ; the suitable argon flow rate for 210 t ladle with double plugs bottom blowing is 200 〜300 L/min.