A Study on Effectiveness of Solid Phase Decarburization of High-Carbon Ferrochrome Powder by Microwave Heating and Conventional Heating
|更新时间:2026-01-21
|
A Study on Effectiveness of Solid Phase Decarburization of High-Carbon Ferrochrome Powder by Microwave Heating and Conventional Heating
Special SteelVol. 35, Issue 5, Pages: 19-22(2014)
作者机构:
1. 太原理工大学材料科学与工程学院,太原,030024
2. 山西工程职业技术学院,太原,030009
作者简介:
基金信息:
DOI:
CLC:
Received:30 April 2014,
Online First:01 September 2022,
Published:01 September 2014
稿件说明:
移动端阅览
郝赳赳, 陈津, 郭丽娜. A Study on Effectiveness of Solid Phase Decarburization of High-Carbon Ferrochrome Powder by Microwave Heating and Conventional Heating[J]. Special Steel, 2014, 35(5): 19-22.
DOI:
郝赳赳, 陈津, 郭丽娜. A Study on Effectiveness of Solid Phase Decarburization of High-Carbon Ferrochrome Powder by Microwave Heating and Conventional Heating[J]. Special Steel, 2014, 35(5): 19-22.DOI:
A Study on Effectiveness of Solid Phase Decarburization of High-Carbon Ferrochrome Powder by Microwave Heating and Conventional Heating
The effect of both method- microwave heating and conventional muffle furnace heating at 900 ~ 1200 ℃ for 0 ~60 min on high-carbon ferrochrome powder (/% : 55.79Cr
32.76Fe
8.16C
2.34Si) decarburizing by solid decarburizer calcium carbonate (96.04% CaCO
3
) has been studied. Results show that in test conditions the effectiveness of solid phase decarburization of high-carbon ferrochrome powder with microwave heating is more obvious than that with conventional heating and the oxidization of materials is serious as heating by conventional method. With microwave heating mixture at 1100 °C for 60 min the decarburization percentage of high-carbon ferrochrome powder is 79.04% to get better deearburization effectiveness and avoid excessive oxidation of materials.