A Study on Optimization of a 20 t Tundish Structure for 3-Strands Casting Based on Hydraulic Simulated Test
|更新时间:2026-01-21
|
A Study on Optimization of a 20 t Tundish Structure for 3-Strands Casting Based on Hydraulic Simulated Test
Special SteelVol. 36, Issue 1, Pages: 1-4(2015)
作者机构:
1. 北京科技大学冶金与生态工程学院,北京,100083
2. 莱芜钢铁股份有限公司特殊钢厂,莱芜,271104
作者简介:
基金信息:
DOI:
CLC:
Received:25 June 2014,
Online First:29 August 2022,
Published:29 August 2015
稿件说明:
移动端阅览
杨凌志, 朱荣, 李超, et al. A Study on Optimization of a 20 t Tundish Structure for 3-Strands Casting Based on Hydraulic Simulated Test[J]. Special Steel, 2015, 36(1): 1-4.
DOI:
杨凌志, 朱荣, 李超, et al. A Study on Optimization of a 20 t Tundish Structure for 3-Strands Casting Based on Hydraulic Simulated Test[J]. Special Steel, 2015, 36(1): 1-4.DOI:
A Study on Optimization of a 20 t Tundish Structure for 3-Strands Casting Based on Hydraulic Simulated Test
The flow field in original tundish with single-line type retaining wall
rectangular guide-flow-hole and level- no dip angle and in improved tundish with V- type retaining wall
Φ80 ~Φ 120 mm round guide-flow-hole and dip angle 0°- 40
°
and adding turbulence inhibitor has been tested and studied by using geometric similarity 1:2.5 water model. It is obtained that the structure of improved tundish with V- type retaining wall +30° angle and diameter Φ80 mm guide-flow- hole + deep disc-lip type edge turbulence inhibitor is optimal
it may prolong the residence time of liquid in tundish and the percentage of dead zone volume of liquid decreases to 10.3% 〜10.9% from 48.16% ~63.06% in original tundish
and is in favor of inclusions in liquid to quick floating off.