Effect of Solid-Solution-Treated Temperature on Structure and Pitting Corrosion Resistance of Maraging Stainless Steel 00Cr13Ni7Co5Mo4W
|更新时间:2026-01-21
|
Effect of Solid-Solution-Treated Temperature on Structure and Pitting Corrosion Resistance of Maraging Stainless Steel 00Cr13Ni7Co5Mo4W
Special SteelVol. 36, Issue 6, Pages: 42-44(2015)
作者机构:
哈尔滨理工大学应用科学学院,哈尔滨,150080
作者简介:
基金信息:
DOI:
CLC:
Received:27 June 2015,
Online First:15 August 2022,
Published:15 August 2015
稿件说明:
移动端阅览
姜越, 黎士强, 张月, et al. Effect of Solid-Solution-Treated Temperature on Structure and Pitting Corrosion Resistance of Maraging Stainless Steel 00Cr13Ni7Co5Mo4W[J]. Special Steel, 2015, 36(6): 42-44.
DOI:
姜越, 黎士强, 张月, et al. Effect of Solid-Solution-Treated Temperature on Structure and Pitting Corrosion Resistance of Maraging Stainless Steel 00Cr13Ni7Co5Mo4W[J]. Special Steel, 2015, 36(6): 42-44.DOI:
Effect of Solid-Solution-Treated Temperature on Structure and Pitting Corrosion Resistance of Maraging Stainless Steel 00Cr13Ni7Co5Mo4W
The effect of solid-solution-treated temperature 1050-1150℃ on structure and corrosion resistance in artificial seawater of maraging steel 00Cr13Ni7Co5Mo4W has been studied by analysis on microstructure
using potentiodynamic polarization curves and uniform corrosion immersion testing. Results show that the solid-solution-treated temperature influences uniformity of structure and grain size of the maraging stainless steel
and then influences the pitting corrosion resistance of steel ; the suitable solid-solution-treated temperature of the maraging stainless steel 00Cr13Ni7Co5Mo4W is 1100 °C
and the annual corrosion rate of the maraging stainless steel 00Cr13Ni7Co5Mo4W solid-solution-treated at 1100℃ for 1 h is only 1.09μm/a