Physical-Mathematical Simulation and Application of Liquid Flow Field in a 35 t Tundish for Three-Strand Unsymmetrical Casting
Special SteelVol. 36, Issue 4, Pages: 1-4(2015)
作者机构:
1. 南京钢铁集团有限公司电弧炉炼钢厂,南京,210035
2. 北京科技大学冶金与生态工程学院,北京,100083
作者简介:
基金信息:
DOI:
CLC:
Received:20 February 2015,
Online First:22 August 2022,
Published:22 August 2015
稿件说明:
移动端阅览
朱守欣, 孙彦辉, 张西超, et al. Physical-Mathematical Simulation and Application of Liquid Flow Field in a 35 t Tundish for Three-Strand Unsymmetrical Casting[J]. Special Steel, 2015, 36(4): 1-4.
DOI:
朱守欣, 孙彦辉, 张西超, et al. Physical-Mathematical Simulation and Application of Liquid Flow Field in a 35 t Tundish for Three-Strand Unsymmetrical Casting[J]. Special Steel, 2015, 36(4): 1-4.DOI:
Physical-Mathematical Simulation and Application of Liquid Flow Field in a 35 t Tundish for Three-Strand Unsymmetrical Casting
According to the research prototype of a 35 t tundish for casting three-strand unsymmetrical 320 mm x 480 mm bloom of GCrl5 bearing steel
with using geometric similarity ratio 1:3 water model combined with mathematical simulation
the effect of different baffle device on liquid flow field in tundish is studied to optimize the tundish flow field and get optimum baffle device. Results show that of original prototype tundish the residence time is smaller and the dead area volume fraction is up to 39. 68% ; adding optimized Y-type baffle the average residence time of three nozzle increases by 29. 51 s
the dead area ratio decreases by 15. 54% and each nozzle is more identical. The pilot production of GCrl5 beari
ng steel in situ show that after tundish optimization the T [O
]
in tundish liquid decreases from original 19. 3 x 10
-6
~26. 3 x 10
-6
average value 22. 7 x 10
-6
to 9. 5 x 10
-6
~ 17. 2 ×10
-6
average 12. 3 x 10
-6
number of inclusions in casting bloom decreases from 12. 0 ~15.3/mm
2
to 6. 8 ~8. 4/mm
2
and the number of > 1. 25 μm inclusions decreases obviously.