Gear Steel 40CrMo Surface Laser Cladding 0.60C-15.25Cr-l. 85Mo Powder process and Its Structure and Properties
Special SteelVol. 37, Issue 1, Pages: 22-24(2016)
作者机构:
1. 宁波中物激光与光电技术研究所,宁波,315100
2. 苏州大学沙钢钢铁学院,苏州,215021
作者简介:
基金信息:
DOI:
CLC:
Received:31 August 2015,
Online First:24 August 2022,
Published:24 August 2016
稿件说明:
移动端阅览
陈磊, 夏志新, 贾帅, et al. Gear Steel 40CrMo Surface Laser Cladding 0.60C-15.25Cr-l. 85Mo Powder process and Its Structure and Properties[J]. Special Steel, 2016, 37(1): 22-24.
DOI:
陈磊, 夏志新, 贾帅, et al. Gear Steel 40CrMo Surface Laser Cladding 0.60C-15.25Cr-l. 85Mo Powder process and Its Structure and Properties[J]. Special Steel, 2016, 37(1): 22-24.DOI:
Gear Steel 40CrMo Surface Laser Cladding 0.60C-15.25Cr-l. 85Mo Powder process and Its Structure and Properties
Based on w inside-laser coaxial powder feedingM technology the surface of steel 40CrMo (/% : 0. 40C
1. 20Cr
0. 25Mo) is laser-clad with iron-base alloy powder (/% : 0. 60C
15. 25Cr
1. 1 ISi
1. 85Mo) to increase surface hardness and get idea wear resistance. The hardness HV0 2 value of steel 40CrMo is 250 while the surface hardness HV
0.2
value by laser cladding is 500. It is available to get better metallurgical binding interface between base metal and coating material by base metal pretreated at 200 °C
and the heat affected zone of base metal and binding interface zone are relatively smaller. Due to quick cooling and alloying effect by larger temperature gradient
the hardness of sample bending zone is higher than other area of laser cladding.