Effect of Diameter of ESR Ingot and Reduction Ratio on Non-Uniformity of Carbide in High-Speed Steel M2
|更新时间:2026-01-21
|
Effect of Diameter of ESR Ingot and Reduction Ratio on Non-Uniformity of Carbide in High-Speed Steel M2
Special SteelVol. 36, Issue 3, Pages: 21-22(2015)
作者机构:
河冶科技股份有限公司,石家庄,052165
作者简介:
基金信息:
DOI:
CLC:
Received:27 December 2014,
Online First:17 August 2022,
Published:17 August 2015
稿件说明:
移动端阅览
邵青立, 谢志彬, 张国平. Effect of Diameter of ESR Ingot and Reduction Ratio on Non-Uniformity of Carbide in High-Speed Steel M2[J]. Special Steel, 2015, 36(3): 21-22.
DOI:
邵青立, 谢志彬, 张国平. Effect of Diameter of ESR Ingot and Reduction Ratio on Non-Uniformity of Carbide in High-Speed Steel M2[J]. Special Steel, 2015, 36(3): 21-22.DOI:
Effect of Diameter of ESR Ingot and Reduction Ratio on Non-Uniformity of Carbide in High-Speed Steel M2
The statistics and regression analysis on the effect of diameter of ESR ingot (Φ250 mm ~ Φ400 mm) and reduction ratio (11. 10 ~92.46) of high speed steel M2 (/% : 0.85 - 0.90C
5.8 - 6.2W
4. 6 - 5.0Mo
3.8- 4.4Cr
1.75 -1.95V) on non-uniformity of carbide in steel products (Φ26 mm - Φ120 mm) have been carried out
and a regression equation to predict the rating of non-uniformity of carbide in products is established. Results show that as reduction ratio is less than 20
with increasing reduction ratio the non-uniformity of carbide in steel decreases markedly
while as reduction ratio is more than 20
with increasing reduction ratio the non-uniformity of carbide in steel decreases lesser; with same reduction ratio the rating of carbide non-uniformity in smaller diameter steel forged and rolled products is smaller.