Effect of Heat Treatment on Structure and Properties of 150 mm Ultra-Heavy Plate of Steel 12Cr2Mo1R for Pressure Vessel
|更新时间:2026-01-21
|
Effect of Heat Treatment on Structure and Properties of 150 mm Ultra-Heavy Plate of Steel 12Cr2Mo1R for Pressure Vessel
Special SteelVol. 36, Issue 6, Pages: 45-48(2015)
作者机构:
作者简介:
基金信息:
DOI:
CLC:
Received:05 June 2015,
Online First:15 August 2022,
Published:15 August 2015
稿件说明:
移动端阅览
何贝, 徐光, 袁清. Effect of Heat Treatment on Structure and Properties of 150 mm Ultra-Heavy Plate of Steel 12Cr2Mo1R for Pressure Vessel[J]. Special Steel, 2015, 36(6): 45-48.
DOI:
何贝, 徐光, 袁清. Effect of Heat Treatment on Structure and Properties of 150 mm Ultra-Heavy Plate of Steel 12Cr2Mo1R for Pressure Vessel[J]. Special Steel, 2015, 36(6): 45-48.DOI:
Effect of Heat Treatment on Structure and Properties of 150 mm Ultra-Heavy Plate of Steel 12Cr2Mo1R for Pressure Vessel
0.015Sn) is melted by EAF then electro-slag remelted to 300 mm x 2 000 mm slab and rolled to 150 mm heavy plate (Opening rolling 1145℃
final rolling 850℃). The static continuous cooling transformation ( CCT) curves and the cooling temperature curves of surface
1/4 thickness and 1/2 thickness ( center) of ultra-heavy plate of steel 12Ci2Mo1R are obtained by thermal simulation test and finite element simulation of temperature field. With normalized at 916 °C for 226 min and tempered at 698 °C for 240 min the structure of hot rolled plate at 1/4 thickness is bainite + minor ferrite
and that at 1/2 thickness is bainite + ferrite
its mechanical properties are yield strength 464 MPa
tensile strength 585 MPa and elongation 22% to meet the requirement of user.