Effect of Fluorite Content on Physical Properties of Mould Powder and Mineralogical Structure of Flux Film
|更新时间:2026-01-21
|
Effect of Fluorite Content on Physical Properties of Mould Powder and Mineralogical Structure of Flux Film
Special SteelVol. 37, Issue 1, Pages: 9-12(2016)
作者机构:
1. 华北理工大学矿业工程学院,唐山,063009
2. 唐钢中厚板有限公司,唐山,063009
作者简介:
基金信息:
DOI:
CLC:
Received:31 August 2016,
Online First:16 August 2022,
Published:16 August 2016
稿件说明:
移动端阅览
王凯强, 韩秀丽, 刘丽娜, et al. Effect of Fluorite Content on Physical Properties of Mould Powder and Mineralogical Structure of Flux Film[J]. Special Steel, 2016, 37(1): 9-12.
DOI:
王凯强, 韩秀丽, 刘丽娜, et al. Effect of Fluorite Content on Physical Properties of Mould Powder and Mineralogical Structure of Flux Film[J]. Special Steel, 2016, 37(1): 9-12.DOI:
Effect of Fluorite Content on Physical Properties of Mould Powder and Mineralogical Structure of Flux Film
According to the issue of easily forming surface longitudinal crack on casting slab of hypo-peritectic steel
the effect of fluorite adding amount on melting temperature
viscosity and average heat flux of mould powder (/% : 29 〜37 cement grog
8 borax
20 quartz sand
15 wollastonite
12 soda
8 ~ 16 fluorite)
and mineralogical structure of flux film has been studied and analyzed. Results show that with increasing fluorite content the crystallization ratio of flux film and cuspidine content in film increase
the wollastonite content in film decreases
and the melting temperature
viscosity and average heat flux of mould powder decrease. It is obtained that adding fluorite content 12% in mould powder could satisfy the requirement on mineralogical structure of flux film for hypo-peritectic steel casting slab and improve the quality of casting slab.