Effect of VIM-ESR-VAR Triplex Melting Process on Cleanliness of Bearing Steel 9Cr88Mo
更新时间:2026-01-21
    • Effect of VIM-ESR-VAR Triplex Melting Process on Cleanliness of Bearing Steel 9Cr88Mo

    • Special Steel   Vol. 39, Issue 1, Pages: 24-27(2018)
    • Received:04 August 2017,

      Online First:30 June 2022,

      Published:30 June 2018

    移动端阅览

  • 何曲波, 王东哲, 刘海定, et al. Effect of VIM-ESR-VAR Triplex Melting Process on Cleanliness of Bearing Steel 9Cr88Mo[J]. Special Steel, 2018, 39(1): 24-27. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Basicity of Tundish Covering Flux on Metallurgy Quality of Ferrite Stainless Steel
Analysis and Control Practice on Typical Defect of N80 Oil Pipe
Modification Effect of Magnesium Treatment on Inclusions in 0.45%C Steel
Effect of Casting Slab Defect on Cold Draw Quality of SWRH82B Steel Wire Coil
Effect of Dynamic Soft Reduction in Casting on Porosity and Inclusions in Heavy Rail of Steel U75V

Related Author

王伟
张润平
任国
杨瑞军
白晋钢
彭自胜
徐景峰
杨敏

Related Institution

武汉科技大学
衡阳华菱钢管有限公司技术中心
南京钢铁股份有限公司
上海大学材料科学与工程学院先进凝固技术中心,省部共建高品质特殊钢冶金与制备国家 重点实验室
东北大学轧制技术与连轧自动化国家重点实验室
0