Analysis of Deformation of Narrow Surface Bulging and Avoiding Measures
更新时间:2026-01-21
    • Analysis of Deformation of Narrow Surface Bulging and Avoiding Measures

    • Special Steel   Vol. 39, Issue 5, Pages: 24-27(2018)
    • Received:03 April 2018,

      Online First:27 May 2022,

      Published:27 May 2018

    移动端阅览

  • 谢长川, 李富帅. Analysis of Deformation of Narrow Surface Bulging and Avoiding Measures[J]. Special Steel, 2018, 39(5): 24-27. DOI:

  •  
  •  