Effect of Anneal Process on Microstructure and Mechanical Properties of Hot Rolled Ferritic Stainless Steel SUS410L
|更新时间:2026-01-21
|
Effect of Anneal Process on Microstructure and Mechanical Properties of Hot Rolled Ferritic Stainless Steel SUS410L
Special SteelVol. 40, Issue 2, Pages: 63-66(2019)
作者机构:
1. 太原理工大学材料与工程学院,太原,030024
2. 太原钢铁(集团)有限公司先进不锈钢材料国家重点实验室,太原,030003
3. 太原科技大学,太原,030024
4. 山西太钢不锈钢股份有限公司冷轧厂,太原,030003
作者简介:
基金信息:
DOI:
CLC:
Received:11 October 2018,
Online First:20 May 2022,
Published:20 May 2019
稿件说明:
移动端阅览
李筱, 卫英慧, 卫争艳, et al. Effect of Anneal Process on Microstructure and Mechanical Properties of Hot Rolled Ferritic Stainless Steel SUS410L[J]. Special Steel, 2019, 40(2): 63-66.
DOI:
李筱, 卫英慧, 卫争艳, et al. Effect of Anneal Process on Microstructure and Mechanical Properties of Hot Rolled Ferritic Stainless Steel SUS410L[J]. Special Steel, 2019, 40(2): 63-66.DOI:
Effect of Anneal Process on Microstructure and Mechanical Properties of Hot Rolled Ferritic Stainless Steel SUS410L
Effect of annealing temperature and holding time on the recrystallization behaviour and mechanical properties of hot rolled stainless steel SUS410L was investigated. Results showed that the hot rolled plate SUS410L did not complete the recrystallization process when annealing temperature was 700 ℃ and holding time was 480 min. The recrystallizai- ton completion time for annealing temperatures of 750 ℃ and 800 ℃ were 120 min and 30 min respectively
grains gradually grew bigger after the completion of recrystallization. To avoid the formation of martensite which decreases the elongation of the material
annealing temperature should not be higher than 800 ℃. Mechanical properties of the material were closely correlated with the recrystallization level. Annealing temperature of 750 ℃ and holding time of 480 min led to the best comprehensive mechanical properties: elongation of 38%
HRB hardness of 67
yield strength of 236 MPa and tensile strength of 441 MPa.