您当前的位置:
首页 >
文章列表页 >
Effect of Heat Treatment Temperature on Microstructure and Properties of Molybdenum Bearing Freeite Stainless Steel 0Crl7Mo2S
更新时间:2026-01-21
    • Effect of Heat Treatment Temperature on Microstructure and Properties of Molybdenum Bearing Freeite Stainless Steel 0Crl7Mo2S

    • Special Steel   Vol. 40, Issue 4, Pages: 48-50(2019)
    • Received:15 February 2019,

      Online First:15 May 2022,

      Published:15 May 2019

    移动端阅览

  • 姜方, 张孟旳, 王刚, et al. Effect of Heat Treatment Temperature on Microstructure and Properties of Molybdenum Bearing Freeite Stainless Steel 0Crl7Mo2S[J]. Special Steel, 2019, 40(4): 48-50. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Heat Treatment,Structure and Properties of High Temperature Stainless Bearing Steel Cr14Mo4
Effect of Heat Treatment Process on Structure and Mechanical Properties of Steel Q345D for Rudder Stock
Heat Treatment, Structure and Properties of High-Strength-Toughness Steel 12Cr2Mo 406 mm x 40.5 nun Tube for High Pressure Boiler
Effect of Heat Treatment on Structure and Properties of Martensite Heat-Resistant Steel 1Cr12Ni3Mo2VN
Effect of Annealing Temperature on Microstructure and Properties of Ferrite Stainless Steel Y0Cr17SiS

Related Author

魏果能
许达
俞峰
范秋梅
付朝波
张永恒
王海珍
张志成

Related Institution

钢铁研究总院结构材料研究所
中原特钢股份有限公司
湖北新冶钢有限公司产品研究所
武汉科技大学国际钢铁研究院
北京航空材料研究院钢与稀贵金属所
0