Process Practice for Production of Φ80 mm Non-Quenched-Tempered Steel 38MnVS6 by 300 mm x 360 mm Continuous Casting Bloom
更新时间:2026-01-21
    • Process Practice for Production of Φ80 mm Non-Quenched-Tempered Steel 38MnVS6 by 300 mm x 360 mm Continuous Casting Bloom

    • Special Steel   Vol. 40, Issue 5, Pages: 21-23(2019)
    • Received:15 March 2019,

      Online First:12 May 2022,

      Published:12 May 2019

    移动端阅览

  • 王春梅, 黄永建, 李双江. Process Practice for Production of Φ80 mm Non-Quenched-Tempered Steel 38MnVS6 by 300 mm x 360 mm Continuous Casting Bloom[J]. Special Steel, 2019, 40(5): 21-23. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

A Study on Dynamics of Al2O3-CaO Base Pre-Molten Refining Slag to Absorb Al2O3 Inclusion
Effect of CaO-Al2O3 Slag Series on Total Oxygen and Sulphur in Gear Steel 20CrMoH
Analysis on Etching of Slag Line Brick of Ladle for Refining Steel Cord of Tyre and Technology Measure for Increasing Service Life
Behavour of Non-metallic Inclusions in Liquid Alloy Steel under High Basicity High A12O3 Slag
Effect of Grain Boundary Segregation of Residual Elements Cu-As-Sn on Intergranular Embrittlement Fracture of Low Alloying Steel

Related Author

赵和明
王新华
谢兵
肖卫军
陈斌姜敏王新华
耿明山
王新华
张炯明

Related Institution

武汉钢铁集团公司第一炼钢厂
北京科技大学冶金与生态工程学院
中国一重能源装备材料科学研究所
江阴兴澄特种钢铁有限公司研究院,江阴
0