Effect of Nb-V Microalloying on Phase Transformation Behavior of High Carbon Steel
更新时间:2026-01-21
    • Effect of Nb-V Microalloying on Phase Transformation Behavior of High Carbon Steel

    • Special Steel   Vol. 40, Issue 4, Pages: 62-65(2019)
    • Received:28 February 2019,

      Online First:15 May 2022,

      Published:15 May 2019

    移动端阅览

  • 沈奎, 江卓俊, 于学森, et al. Effect of Nb-V Microalloying on Phase Transformation Behavior of High Carbon Steel[J]. Special Steel, 2019, 40(4): 62-65. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

1

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Influence of V Content on Natural Ageing Properties of High Nitrogen Steel 20MnSi
Precipitate Behavior of Second Phase and Structure of Annealed 1.5 mm Cold Rolling Sheet of Nb-Ti Microalloy High Strength Steel
Effect of Finished Rolling Cooling Rate on Structure of Microalloy Non Quenched-Tempered Steel 34Mn2VN
Effect of Solution Temperature on Structure and Properties of 022Cr22Ni5Mo3N Duplex Stainless Steel
Effect of Quenching and Partitioning(Q & P)Process on Structure and Mechanical Properties of Steel 25Si2Ni3

Related Author

杨吉春
张剑
周莉
栗宏伟
刘浩
陈晓
李平和
郑红

Related Institution

内蒙古科技大学材料与冶金学院
武汉科技大学材料与冶金学院
武汉钢铁公司技术中心
钢铁研究总院
北京科技大学材料学院
0