Development of X80M Pipeline Steel of 30.8 mm x 4 342 mm Wide Plate for Low Temperature and High Pressure Service at Nanjing Iron and Steel Co Ltd
更新时间:2026-01-21
    • Development of X80M Pipeline Steel of 30.8 mm x 4 342 mm Wide Plate for Low Temperature and High Pressure Service at Nanjing Iron and Steel Co Ltd

    • Special Steel   Vol. 40, Issue 6, Pages: 42-45(2019)
    • Received:17 May 2019,

      Online First:11 May 2022,

      Published:11 May 2019

    移动端阅览

  • 翟冬雨, 杜海军, 姜金星. Development of X80M Pipeline Steel of 30.8 mm x 4 342 mm Wide Plate for Low Temperature and High Pressure Service at Nanjing Iron and Steel Co Ltd[J]. Special Steel, 2019, 40(6): 42-45. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

No data

Related Author

No data

Related Institution

No data
0