Analysis and Improvement Measures on Band Structure Formation of 42CrMoA Rolled Steel with 120 t BOF-LF-RH-Φ300 mm CC-CR Flowsheet
更新时间:2026-01-21
    • Analysis and Improvement Measures on Band Structure Formation of 42CrMoA Rolled Steel with 120 t BOF-LF-RH-Φ300 mm CC-CR Flowsheet

    • Special Steel   Vol. 42, Issue 4, Pages: 81-83(2021)
    • Received:18 January 2021,

      Online First:09 March 2022,

      Published:09 March 2021

    移动端阅览

  • 介瑞华. Analysis and Improvement Measures on Band Structure Formation of 42CrMoA Rolled Steel with 120 t BOF-LF-RH-Φ300 mm CC-CR Flowsheet[J]. Special Steel, 2021, 42(4): 81-83. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Isothermal Temperature on Banded Structure in Low Carbon Gear Steel
Low Temperature Impact Toughness of Hot Rolled Steel Sheet Pile SY390BZ
Analysis on Surface Crack Formation Mechanism for Crankshaft Forgings of Steel 42CrMo and Process Improvement
Analysis on Capillary Crack Defect in Anchor Steel CM690 and Process Improvement

Related Author

李博鹏
陈长西
周立新
张跃尊
黄运华
蔡珍
杜美文
周剑华

Related Institution

北京科技大学1新金属材料国家重点实验室
材料科学与工程学院
湖北新冶钢有限公司
武汉科技大学材料与冶金学院
武汉钢铁(集团)公司研究院
0