Effect of Rough Rolling Process on Microstructure and Mechanical Properties of 700 MPa Ti Micro-Alloyed High-Strength Steel
更新时间:2026-01-21
    • Effect of Rough Rolling Process on Microstructure and Mechanical Properties of 700 MPa Ti Micro-Alloyed High-Strength Steel

    • Special Steel   Vol. 42, Issue 1, Pages: 61-65(2021)
    • Received:09 July 2020,

      Online First:11 April 2022,

      Published:11 April 2021

    移动端阅览

  • 陈述. Effect of Rough Rolling Process on Microstructure and Mechanical Properties of 700 MPa Ti Micro-Alloyed High-Strength Steel[J]. Special Steel, 2021, 42(1): 61-65. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Structure and Mechanical Properties of Medium and Heavy Plate of Ti Microalloyed Q345D Steel
Numerical Simulation and Process Improvement on Rough Rolling of 250 mm x 280 mm Cast Bloom to 138 mm x 150 nun Billet of GCr15 Bearing Steel

Related Author

周家林
黄高
向上
潘成刚
赖春明
胡唐国
苟复钢
王青海

Related Institution

武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
武汉钢铁股份有限公司
西宁特殊钢集团有限责任公司1精品小棒线分厂,2股份公司
0