Influence of Boronizing Process on Properties of Hot Forging Die Steel 45CrNiMoV for Automobile
更新时间:2026-01-21
    • Influence of Boronizing Process on Properties of Hot Forging Die Steel 45CrNiMoV for Automobile

    • Special Steel   Vol. 42, Issue 1, Pages: 57-60(2021)
    • Received:03 July 2020,

      Online First:11 April 2022,

      Published:11 April 2021

    移动端阅览

  • 李小明. Influence of Boronizing Process on Properties of Hot Forging Die Steel 45CrNiMoV for Automobile[J]. Special Steel, 2021, 42(1): 57-60. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Boron on Hot Workability,Structure and Mechanical Properties of Austenite Heat Resistant Steel TP347H
Effect of Recycled Smelting Number of Times on Chemical Composition, Structure and Mechanical Properties of Recycled Alloy M17
Structure and Properties of 323.9  mmx14.2 mm 15NiCuMoNb5-6-4 Steel Seamless Tube for Nuclear Power Station
Progress of Research on Performance of Passive Films of Stainless Steels
Effect of Quenching-Tempering Process on Microstructure and Properties of Micro-Alloying Q960E Steel 70 mm Thickness Plate

Related Author

楼琅洪
张匀
孙晓峰
董加胜
谷力功
王国亮
肖功业
桂艳

Related Institution

中国科学院金属研究所
天津钢管集团股份有限公司
华南理工大学材料科学与工程学院
河钢股份有限公司邯郸分公司技术中心
东北大学材料与冶金学院
0