您当前的位置:
首页 >
文章列表页 >
Effect of Normalizing Preheat Treatment on Structure and Properties of 42CrMo Forging Crankshaft Steel after Quenching and Tempering Treatment
更新时间:2026-01-21
    • Effect of Normalizing Preheat Treatment on Structure and Properties of 42CrMo Forging Crankshaft Steel after Quenching and Tempering Treatment

    • Special Steel   Vol. 41, Issue 4, Pages: 26-29(2020)
    • Received:07 January 2020,

      Online First:27 April 2022,

      Published:27 April 2020

    移动端阅览

  • 李康丽, 李永志, 孙国栋. Effect of Normalizing Preheat Treatment on Structure and Properties of 42CrMo Forging Crankshaft Steel after Quenching and Tempering Treatment[J]. Special Steel, 2020, 41(4): 26-29. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Present Status and Development Tendency of Patented Technology for High Strength Oil Well Tubing Steels
Production Practice of Φ219.1mm x9.5mm Anti-Hydrogen Sulfide Corrosion Seamless Pipe Line Steel Tube X52QS
Effect of Quenching and Tempering Treatment on Structure and Mechanical Properties of 22MnCrNiMo Steel Flash Weld Zone

Related Author

牟昊
陈妍
齐殿威
丁伟
吴美庆
王学敏
邓叙燕
李健强

Related Institution

鞍钢股份公司技术中心,鞍山9
达力普石油专用管有限公司技术中心
河北省石油专用管工程技术研究中心
江苏科技大学材料科学与工程学院
0