您当前的位置:
首页 >
文章列表页 >
Water Model Experiment on Interaction Between Innovated Double-Structure Oxygen Lance and Converter Molten Pool
更新时间:2026-01-21
    • Water Model Experiment on Interaction Between Innovated Double-Structure Oxygen Lance and Converter Molten Pool

    • Special Steel   Vol. 41, Issue 2, Pages: 6-9(2020)
    • Received:25 October 2019,

      Online First:21 April 2022,

      Published:21 April 2020

    移动端阅览

  • 张国新, 刘广强, 刘坤, et al. Water Model Experiment on Interaction Between Innovated Double-Structure Oxygen Lance and Converter Molten Pool[J]. Special Steel, 2020, 41(2): 6-9. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Experiment on Optimum Location of Bottom Nozzle in a 130 t Argon Stirred Ladle by Water Model
Study of Water Model on Mixing Characteristics of Flow Field in CAS Ladle with Deep Inserting Snorkel
Experimental Study on Water Model for a 50 t Top and Bottom Combined Blown Converter at Tangsteel
A Study on Physical Simulation for Liquid Flow in a New-Type Ladle at Xingcheng Special Steel
A Study on Water Model for Optimum Location of 150 t Ladle Bottom Blowing Argon Nozzle

Related Author

幸伟
倪红卫
沈巧珍
张华
何环宇
何平
干磊
曾亚南

Related Institution

武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
钢铁研究总院冶金工艺研究所,北京1
河北理工大学冶金与能源学院,唐11J
唐山钢铁股份有限公司
兴澄特种钢铁有限公司,江阴
0