Analysis of Cogging Cracking and Process Improvement of Ni-Base Corrosion Resistant Alloy N10276
更新时间:2026-01-21
    • Analysis of Cogging Cracking and Process Improvement of Ni-Base Corrosion Resistant Alloy N10276

    • Special Steel   Vol. 43, Issue 2, Pages: 36-39(2022)
    • Received:15 July 2021,

      Online First:10 June 2022,

      Published:10 June 2022

    移动端阅览

  • 王鑫潮, 王岩, 李吉东. Analysis of Cogging Cracking and Process Improvement of Ni-Base Corrosion Resistant Alloy N10276[J]. Special Steel, 2022, 43(2): 36-39. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Thermodynamic Calculation and Analysis on Equilibrium Phases Transition in T122 Heat-Resistant Steel
Thermodynamic Calculation and Analysis on Equilibrium Phases Transformation in SA508-3 Steel
Effect of Aging Treatment on Microstructure and Pitting Corros-ion Property of 00Cr29Ni6Mo2N Super Duplex Stainless Steel
Effect of Aging Treatment on Mechanical Properties and Microstrure of 05Crl7Ni4Cu4Nb Martensitic Precipitation Hardening Stainless Steel
Effect of Niobium on Mechanical Properties of a New Ni-Cr-Fe Nickel Base Alloy

Related Author

刘正东
程世长
杨钢
谢建新
曹金荣
陈红宇
刘正东
林肇杰

Related Institution

钢铁研究总院结构材料研究所
昆明理工大学材料与冶金工程学院
内蒙古科技大学材料与冶金学院
太钢不锈钢股份有限公司技术中心
冶金工业过程系统科学湖北省重点实验室
0