Research and Development on ML45Mn2  Cold Heading Steel Wire Rod
更新时间:2026-01-21
    • Research and Development on ML45Mn2  Cold Heading Steel Wire Rod

    • Special Steel   Vol. 43, Issue 4, Pages: 28-31(2022)
    • Received:04 November 2021,

      Online First:12 August 2022,

      Published:12 August 2022

    移动端阅览

  • 周国子, 李为龙. Research and Development on ML45Mn2  Cold Heading Steel Wire Rod[J]. Special Steel, 2022, 43(4): 28-31. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

3

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Controlled Rolling and Controlled Cooling and Cooling Bed Heat Preservation Process on Mechanical Properties of 42CrMo Steel φ50 mm Rolled Bar
Thermal Simulation Study on Controlled Rolling and Cooling Process for Quality Spring 60Si2CrVAT
Development of Energy Saving Cold Heading Steels by 100 t EAF-LF-CC-CR Flow Sheet
Production Practice of Nb-Ti Microalloying and Containing Cr Steel J55 for Oil Casing Tube
Effect of Grain Size on Impact Energy of Φ140 mm Products of Steel Q345E at -40 ℃ and Rolling Process Improvement

Related Author

金启邦
孙世平
王青海
年国恩
鲜奋强
刘雅政
黄学启
崔娟

Related Institution

技术中心
股份公司
西宁特殊钢集团有限责任公司1精品小棒线分厂
北京科技大学材料科学与工程学院
沙钢钢铁研究院,张家港
0