Microstructure and Properties of Q500qE Low Yield Ratio High Strength Steel 60 mm Thickness Plate
更新时间:2026-01-21
    • Microstructure and Properties of Q500qE Low Yield Ratio High Strength Steel 60 mm Thickness Plate

    • Special Steel   Vol. 43, Issue 5, Pages: 74-77(2022)
    • Received:26 May 2022,

      Online First:29 September 2022,

      Published:29 September 2022

    移动端阅览

  • 孙宪进, 杜鹏举, 赵乾. Microstructure and Properties of Q500qE Low Yield Ratio High Strength Steel 60 mm Thickness Plate[J]. Special Steel, 2022, 43(5): 74-77. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Tempering Process on Microstructure and Mechanical Properties of Dual Phase High Strength Bridge Steel with Low Yield Ratio

Related Author

Du Pengju
Yu Xinyun
Sun Xianjin
Liu Guanyou

Related Institution

Jiangyin Xincheng Special Steel Works Co., Ltd., Jiangyin
0