钢包自开是影响连铸顺行的关键环节,同时也是影响钢液洁净度的重要因素。钢包无法自开则需烧 氧引流,破坏烧结层,会导致钢液大量增氧,严重降低钢液洁净度。为了提高钢包自开率以改善钢液洁净度,总结了引流砂种类、粒度、含水量、填加剂、填加方式、水口座砖形状特点以及引流砂与钢液反应等因素对钢包自开率的 影响,其中粒度在0.5-1.4 mm
The ladle self-opening is a key step that affects the smooth running of continuous casting. Meantime
it is an important factor that affects the cleanliness of molten steel. If the ladle can not be opened by itself
it will have to use oxygen lance for introducing liquid flowing to destroy the sintered layer
but this will lead to a large amount of oxygenation of steel and seriously damage the cleanliness of the molten steel. In order to improve the cleanliness of molten steel by increasing ladle self-opening rate
the influences of filler sand types
particle sizes
water content
additives
adding methods
shape characteristics of nozzle base brick and the reaction between filler sand and molten steel on the self-opening rate of ladle are summarized
among them
the filler sand with particle size is 0. 5 ~ 1.4 mm contained appropriate amount of coarse rounded particles
filler graphite content 2% 〜4% and water content less than 0. 15% has a higher opening rate.