您当前的位置:
首页 >
文章列表页 >
Mathematical Simulation of Flow Field Characteristics of Molten Steel with Bottom Argon Blowing Process in 180 t Ladle
更新时间:2026-01-21
    • Mathematical Simulation of Flow Field Characteristics of Molten Steel with Bottom Argon Blowing Process in 180 t Ladle

    • Special Steel   Vol. 42, Issue 5, Pages: 6-10(2021)
    • Received:01 March 2021,

      Online First:12 December 2022,

      Published:12 December 2021

    移动端阅览

  • 杨亚迪, 赵晶, 崔剑征. Mathematical Simulation of Flow Field Characteristics of Molten Steel with Bottom Argon Blowing Process in 180 t Ladle[J]. Special Steel, 2021, 42(5): 6-10. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

1

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Nu merical Simulation of Temperature Field of 304 Stainless Steel Rod and Wire Hot Continuous Rolling
Numeric Simulation of Three-Dimensional Flow Field of Molten Steel in a Mould with High Efficiency Inner and Outer Couple Cooling
Numerical Simulation of Fluid Field of Molten Steel in Mold for 280 mm×380 mm Billet Concasting
Physical and Mathematical Study on Flow Control Device of Tundish for 5-Strand billet Casting at Chongqing Steel
Numerical Simulation of Flow Field in Mould for Slab Continuous Casting and Optimal Operation

Related Author

廖舒纶
于永泗
张立文
原思宇
江国栋
甑玉
郭书奇
崔小朝

Related Institution

太原科技大学工程力学系
鞍山钢铁集团技术中心
辽宁科技大学材料学院
重庆大学材料科学与工程学院
重庆钢铁集 团有 限公 司
0