Effect of Casting Slab Shot Blasting Process on Surface Quality of 430 Ferritic Stainless Steel Rolled Coil Plate
更新时间:2026-01-21
    • Effect of Casting Slab Shot Blasting Process on Surface Quality of 430 Ferritic Stainless Steel Rolled Coil Plate

    • Special Steel   Vol. 43, Issue 5, Pages: 47-50(2022)
    • Online First:28 September 2022,

      Published:28 September 2022

    移动端阅览

  • 李鹏飞, 翟俊, 杨永杰. Effect of Casting Slab Shot Blasting Process on Surface Quality of 430 Ferritic Stainless Steel Rolled Coil Plate[J]. Special Steel, 2022, 43(5): 47-50. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Optimizing Mold Powder to Improve the Surface Quality of 38CrMoAl High Aluminum Steel Continuous Casting Billet
Effect of Spray Combined Cooling Control Technology on Microstructure and Properties of Spring Steel 54SiCr6
Influence of Additive Composition of Protective Slag on Surface Quality of M2 High Speed Steel Mold Ingot
Influence Factors on Phosphating Quality of GCrl5 Bearing Steel Coil
Effect of Center Line Shrinkage of 0180 mm Casting Bloom of Steel Grade B on Quality of 168 mm x 7 mm Tube Rolled by Accu-Roll

Related Author

Fang Yong
Zong Hao
Hu Jinzhao
李慎松
金维松
于斌
王海兵
胡茂会

Related Institution

Jiangyin Xingcheng Special Steel Co.Ltd., Jiangyin
Second rolling steel branch, Jiangyin Xingcheng Special Steel Co., Ltd., Jiangyin
Steelmaking branch plant, Heye Science and Technology Co., Ltd.
东北特殊钢集团有限责任公司
攀钢集团成都钢钥有限公司
0