Study on Precipitation and Dissolution Behavior of δ Phase in GH4169 Alloy
更新时间:2026-01-21
    • Study on Precipitation and Dissolution Behavior of δ Phase in GH4169 Alloy

    • Special Steel   Vol. 42, Issue 5, Pages: 21-25(2021)
    • Received:20 March 2021,

      Online First:12 December 2022,

      Published:12 December 2021

    移动端阅览

  • 白亚冠, 李红梅, 韩秀栋, et al. Study on Precipitation and Dissolution Behavior of δ Phase in GH4169 Alloy[J]. Special Steel, 2021, 42(5): 21-25. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Electromagnetic Stirring on Solidification Structure of 1 t Electroslag Remelting Ingot of Alloy GH4169

Related Author

吕达
张雲飞
张福利
韩彦光
任帅
崔毅
白丽娟

Related Institution

河北钢铁技术研究总院
0