Hot Deformation Behavior and Microstructure Evolution of N08800 Iron-Nickel Base Alloy
更新时间:2026-01-21
    • Hot Deformation Behavior and Microstructure Evolution of N08800 Iron-Nickel Base Alloy

    • Special Steel   Vol. 42, Issue 5, Pages: 16-20(2021)
    • Received:10 February 2021,

      Online First:02 February 2023,

      Published:02 February 2021

    移动端阅览

  • 李莎, 赵振铎, 王贵平. Hot Deformation Behavior and Microstructure Evolution of N08800 Iron-Nickel Base Alloy[J]. Special Steel, 2021, 42(5): 16-20. DOI:

  •  
  •  