您当前的位置:
首页 >
文章列表页 >
Internal Surface Crack Defect Analysis and Process Improvement of SUS410 Semi-Martensite Stainless Steel Thick Wall Seamless Tube
更新时间:2026-01-21
    • Internal Surface Crack Defect Analysis and Process Improvement of SUS410 Semi-Martensite Stainless Steel Thick Wall Seamless Tube

    • Special Steel   Vol. 42, Issue 5, Pages: 46-48(2021)
    • Received:02 March 2021,

      Online First:03 February 2023,

      Published:03 February 2021

    移动端阅览

  • 唐科, 彭俊, 付克刚, et al. Internal Surface Crack Defect Analysis and Process Improvement of SUS410 Semi-Martensite Stainless Steel Thick Wall Seamless Tube[J]. Special Steel, 2021, 42(5): 46-48. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Cr Content on the Microstructure and Mechanical Properties of 0.03C-XCr-14Ni-2.3Mo-0.35Nb-Fe Austenitic Stainless Steel
Effect of Progressive Solid Solution Treatment on the Structure and Properties of 316H Stainless Steel

Related Author

Xu Yang
Yi Haoyu
Jiang Yuefeng
Ma Yingche
Liang Rui
Liang Tian
Wang Ping
Jing Xue

Related Institution

Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education, Northeastern University
Key Laboratory of Nuclear Materials and Safety Evaluation, Institute of Metal Research, Chinese Academy of Sciences
CGN Nuclear Power Research Institute Co., Ltd.
Shi Changxu Innovation Materials Research Center, Institute of Metal Research, Chinese Academy of Sciences
Metallurgical College, Northeastern University
0