Study on Control Cooling Technology fbr Improving Strength of Q355B Hot Rolling H-Beam Steel
更新时间:2026-01-21
    • Study on Control Cooling Technology fbr Improving Strength of Q355B Hot Rolling H-Beam Steel

    • Special Steel   Vol. 43, Issue 2, Pages: 51-54(2022)
    • Received:14 July 2021,

      Online First:10 June 2022,

      Published:10 June 2022

    移动端阅览

  • 徐正彪, 王延苹, 刘瑞刚, et al. Study on Control Cooling Technology fbr Improving Strength of Q355B Hot Rolling H-Beam Steel[J]. Special Steel, 2022, 43(2): 51-54. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Research and Application of Ferrite Rolling at Home and Abroad
Effect of Controlling Cooling on Structure and Properties of Wire Coil of High Carbon Steel SWRH82B-1V
Effect of Recycling Phase Transformation on Grain Refinement and Mechanical Properties of Maraging Stainless Steel 00Cr13Ni7Co5Mo4Ti

Related Author

徐光
徐楚韶
赵嘉蓉
华蔚
徐震
宋金玲
张驰
江来珠

Related Institution

武汉科技大学
重庆大学材料科学与工程学院
宝山钢铁股份有限公司研究院
哈尔滨理工大学应用科学学院
0