您当前的位置:
首页 >
文章列表页 >
Analysis and Process Improvement on Defects of Broken Bits Dropping Out from Fracture Surface for Microalloying C70S6 Expansion-Broken Connecting Rods
更新时间:2026-01-21
    • Analysis and Process Improvement on Defects of Broken Bits Dropping Out from Fracture Surface for Microalloying C70S6 Expansion-Broken Connecting Rods

    • Special Steel   Vol. 43, Issue 4, Pages: 50-54(2022)
    • Received:18 December 2021,

      Online First:16 August 2022,

      Published:16 August 2022

    移动端阅览

  • 邓向阳, 谢有, 李仕超. Analysis and Process Improvement on Defects of Broken Bits Dropping Out from Fracture Surface for Microalloying C70S6 Expansion-Broken Connecting Rods[J]. Special Steel, 2022, 43(4): 50-54. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

No data

Related Author

No data

Related Institution

No data
0