Numerical Simulation of Effect of Continuous Casting Process Parameters on Solidiflcation Structure of 20CrMnTi Gear Steel 150 mm x 150 mm Billet and Production Application
|更新时间:2026-01-21
|
Numerical Simulation of Effect of Continuous Casting Process Parameters on Solidiflcation Structure of 20CrMnTi Gear Steel 150 mm x 150 mm Billet and Production Application
Special SteelVol. 43, Issue 2, Pages: 16-20(2022)
作者机构:
1. 北京科技大学钢铁共性技术协同创新中心,北京,100083
2. 江苏沙钢集团淮钢特钢有限公司总工办,淮安,223002
作者简介:
基金信息:
DOI:
CLC:
Received:24 July 2021,
Online First:09 June 2022,
Published:09 June 2022
稿件说明:
移动端阅览
史建凯, 岳峰, 田儒良, et al. Numerical Simulation of Effect of Continuous Casting Process Parameters on Solidiflcation Structure of 20CrMnTi Gear Steel 150 mm x 150 mm Billet and Production Application[J]. Special Steel, 2022, 43(2): 16-20.
DOI:
史建凯, 岳峰, 田儒良, et al. Numerical Simulation of Effect of Continuous Casting Process Parameters on Solidiflcation Structure of 20CrMnTi Gear Steel 150 mm x 150 mm Billet and Production Application[J]. Special Steel, 2022, 43(2): 16-20.DOI:
Numerical Simulation of Effect of Continuous Casting Process Parameters on Solidiflcation Structure of 20CrMnTi Gear Steel 150 mm x 150 mm Billet and Production Application
In order to improve the solidification structure of steel 20CrMnTi billet
based on the CAFE model in ProCAST software
the solidification structure is numerically simulated
and the effects of different superheat of molten steel
casting speed of billet and secondary cooling water ratio on the solidification structure are studied. The simulation results show that with decreasing the superheat of molten steel
and increasing cast speed
and decreasing the specific water a- mount of secondary cooling can increase the equiaxed grain ratio and refine the grain size of the billet
and the superheat of molten steel has the most influence on it; the equiaxed grain rate increases by 3. 7% with the decrease of superheat by 10°C ;the equiaxed grain ratio of the casting billet increases by 1. 8% on average when the cast speed increases by 0.1 m/ min; and the equiaxed grain ratio of the billet increases by 1. 65% when the specific water amount decreases by 0. 1 L/kg. Production application shows that with superheat of molten steel 30 °C,as cast speed decreases from original 2. 2 m/min to 2. 1 m/min
secondary cooling specific water amount inceases from 0. 6 L/kg to 0. 7 L/kg