Effect of Al Content and Cr-Mo Microalloying on Crack Formation in 37Mn Steel Φ350 mm Continuous Cast Bloom
更新时间:2026-01-21
    • Effect of Al Content and Cr-Mo Microalloying on Crack Formation in 37Mn Steel Φ350 mm Continuous Cast Bloom

    • Special Steel   Vol. 43, Issue 6, Pages: 83-88(2022)
    • DOI:10.20057/j.1003-8620.2022-00004    

      CLC:
    • Received:01 September 2022,

      Online First:21 November 2022,

      Published:21 November 2022

    移动端阅览

  • 扈立, 侯强, 范淑敏, et al. Effect of Al Content and Cr-Mo Microalloying on Crack Formation in 37Mn Steel Φ350 mm Continuous Cast Bloom[J]. Special Steel, 2022, 43(6): 83-88. DOI: 10.20057/j.1003-8620.2022-00004.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

An Analysis on Formation and Distribution of Cracks in 2 mm 304 Stainless Steel Concasting Thin Strip
A Study on Hot Ductility of Q235B Steel Thin Slab
Analysis on Hot Heading Crack of Non-Quenched and Tempered Steel F45MnVS and Improved Measures of Process

Related Author

王振敏
方圆
张跃
黄运华
齐俊杰
孙彦辉
赵长亮
成小军

Related Institution

北京科技大学材料科学与工程学院
鞍山科技大学材料科学与工程学院
上海宝钢集团公司
北京科技大学冶金与生态工程学院
湖南华菱涟源钢铁有限公司
0