Optimization of “C-P-T” Co-operating Control Process in Converter Steelmaking for GCr15 Bearing Steel
更新时间:2026-01-21
    • Optimization of “C-P-T” Co-operating Control Process in Converter Steelmaking for GCr15 Bearing Steel

    • Special Steel   Vol. 43, Issue 6, Pages: 54-59(2022)
    • DOI:10.20057/j.1003-8620.2022-00010    

      CLC:
    • Received:30 March 2022,

      Online First:22 November 2022,

      Published:22 November 2022

    移动端阅览

  • 肖丙政, 谢海平, 魏刚武, et al. Optimization of “C-P-T” Co-operating Control Process in Converter Steelmaking for GCr15 Bearing Steel[J]. Special Steel, 2022, 43(6): 54-59. DOI: 10.20057/j.1003-8620.2022-00010.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

2

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Characteristics and Evolution of Non-metallic Inclusions in Metallurgical Production of GCr15 Bearing Steel
Research Progress and Prospects of Ultra-High Strength Steel
Effect on Fatigue Failure Behavior Induced by Inclusions in GCr15 Bearing Steel Under Different Metallurgical Processes
Key Smelting Processes and Quality Control Strategies of Nickel-based Superalloys
Key Metallurgical Technologies for Smelting 1Cr13 Stainless Steel via ANS-OB Process

Related Author

Li Weitao
Wu Fapu
Yu Guangfu
Wang Huajun
Wang Kaimin
Jia Xingyu
Tang Haiyan
Hu Chundong

Related Institution

School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing
Weifang Special Steel Group Co., Ltd.
State Key Laboratory of Materials for Advanced Nuclear Energy
School of Materials Science and Engineering,Shanghai University
Zhejiang Research Institute for Advanced Machine Component Materials
0