Optimization of Production Process of 16MnCrS5 Steel Bar for Precision Turning
更新时间:2026-01-21
    • Optimization of Production Process of 16MnCrS5 Steel Bar for Precision Turning

    • Special Steel   Vol. 44, Issue 2, Pages: 48-51(2023)
    • DOI:10.20057/j.1003-8620.2022-00068    

      CLC:
    • Received:22 September 2022,

      Online First:27 March 2023,

      Published:27 March 2023

    移动端阅览

  • 张光鸿, 龙开西, 何英武, et al. Optimization of Production Process of 16MnCrS5 Steel Bar for Precision Turning[J]. Special Steel, 2023, 44(2): 48-51. DOI: 10.20057/j.1003-8620.2022-00068.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

1

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Nioblum on Microstructure and Properties of 65Mn High Carbon Cutting Tool Steel
Dynamic CCT Curve and Microstructures of Antimony Micro-alloyed HRB500 Low-temperature Steel
Ultra-High Strength 50SiMnCr Spring Flat Steel and Its Continuous Cooling Transformation Behavior
Development of Pre-hardened and Ultra-thick 1.2311 Steel Plate Used for Plastic Mold Steel
Influence of Quenching Process on the Microstructure Evolution and Hardness of A514CrQ Rack Steel

Related Author

Yang Yu
Wang Tianxiao
Song Xiaoming
Xu Cheng
Wang Runqi
Pan Xiquan
Zhang ke
Zhang Mingya

Related Institution

State Key Laboratory of Metallic Materials for Marine Equipment and Applications
Angang Steel Co., Ltd.
School of Materials Science and Engineering, Dalian University of Technology Liaoning
Technical Center, Hunan Valin Xiangtan Iron and Steel Co., Ltd.
Anhui university of Technology
0