Improving Sulfide Morphology of Non-quenched and Tempered Steel 38MnVS6 for Automobile Crankshaft by Tellurium Treatment
更新时间:2026-01-21
    • Improving Sulfide Morphology of Non-quenched and Tempered Steel 38MnVS6 for Automobile Crankshaft by Tellurium Treatment

    • Special Steel   Vol. 43, Issue 6, Pages: 79-82(2022)
    • DOI:10.20057/j.1003-8620.2022-00088    

      CLC:
    • Received:26 August 2022,

      Online First:21 November 2022,

      Published:21 November 2022

    移动端阅览

  • 轩康乐, 刘栋林, 俞杰, et al. Improving Sulfide Morphology of Non-quenched and Tempered Steel 38MnVS6 for Automobile Crankshaft by Tellurium Treatment[J]. Special Steel, 2022, 43(6): 79-82. DOI: 10.20057/j.1003-8620.2022-00088.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Modification Effect of Magnesium Treatment on Inclusions in 0.45%C Steel

Related Author

朱浩然
刘年富
周蕾
付建勋

Related Institution

上海大学材料科学与工程学院先进凝固技术中心,省部共建高品质特殊钢冶金与制备国家 重点实验室
南京钢铁股份有限公司
0