Effect of Chromium Alloying on Microstructure  and Properties of C82D2Cr Steel Cord Wire Rod
更新时间:2026-01-21
    • Effect of Chromium Alloying on Microstructure  and Properties of C82D2Cr Steel Cord Wire Rod

    • Special Steel   Vol. 44, Issue 1, Pages: 101-104(2023)
    • DOI:10.20057/j.1003-8620.2022-00097    

      CLC:
    • Received:26 July 2022,

      Online First:31 January 2023,

      Published:31 January 2023

    移动端阅览

  • 李麦麦, 袁相坤, 高永彬, et al. Effect of Chromium Alloying on Microstructure  and Properties of C82D2Cr Steel Cord Wire Rod[J]. Special Steel, 2023, 44(1): 101-104. DOI: 10.20057/j.1003-8620.2022-00097.

  •  
  •  