Comparison and Analysis of Secondary Oxidation Degree in the First Heat of Continuous Casting
更新时间:2026-01-21
    • Comparison and Analysis of Secondary Oxidation Degree in the First Heat of Continuous Casting

    • Special Steel   Vol. 44, Issue 2, Pages: 56-60(2023)
    • DOI:10.20057/j.1003-8620.2022-00103    

      CLC:
    • Received:15 September 2022,

      Online First:27 March 2023,

      Published:27 March 2023

    移动端阅览

  • 张新文, 施嘉凯, 汪德伟, et al. Comparison and Analysis of Secondary Oxidation Degree in the First Heat of Continuous Casting[J]. Special Steel, 2023, 44(2): 56-60. DOI: 10.20057/j.1003-8620.2022-00103.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Current on the Cleanliness of Electroslag Ingots During Low Frequency Electroslag Remelting
Effect on Fatigue Failure Behavior Induced by Inclusions in GCr15 Bearing Steel Under Different Metallurgical Processes
Effect of Refining Slag Basicity on the Molten Steel Cleanliness of GCr15SiMn Bearing Steel
High Temperature Mechanical Properties and Fracture Mechanism of 9Cr-2W-3Co Martensitic Heat-resistant Steel
Effect of LF Soft Bubbling Time on Inclusions in Tire Cord Steel LX82 A

Related Author

Wang Bingjie
Wang Yu
Xiang Miaomiao
Shi Xiaofang
Chang Lizhong
Wang Zheng
Chen feng
Shi Tao

Related Institution

School of Metallurgical Engineering, Anhui University of Technology
Jiangying Xingcheng Special Steel Works Co., Ltd., Jiangying
School of Metallurgy and Ecological Engineering, University of Science and Technology Beijing
Changzhou Baoling Heavy & Industrial Machinery Co., Ltd.
Daye Special Steel Co., Ltd.
0