Development Status of Continuous Casting Process for High-Carbon and High-Alloy Tool and Die Steel
更新时间:2026-01-21
    • Development Status of Continuous Casting Process for High-Carbon and High-Alloy Tool and Die Steel

    • Special Steel   Vol. 43, Issue 6, Pages: 66-72(2022)
    • DOI:10.20057/j.1003-8620.2022-00104    

      CLC:
    • Received:26 August 2022,

      Online First:21 November 2022,

      Published:21 November 2022

    移动端阅览

  • 姚健, 朱喜达, 刘宇, et al. Development Status of Continuous Casting Process for High-Carbon and High-Alloy Tool and Die Steel[J]. Special Steel, 2022, 43(6): 66-72. DOI: 10.20057/j.1003-8620.2022-00104.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

2

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Production Process Practice of Cold-working Die Steel (Cr12MoV) Produced by Short Process
Optimizing Mold Powder to Improve the Surface Quality of 38CrMoAl High Aluminum Steel Continuous Casting Billet
Effects of LB/M Duplex Phase Heat Treatment on Microstructure and Mechanical Properties of Cold Working Die Steel DC53
Research on a Steel Leakage Prediction Model Based on One vs Rest Genetic Algorithm Optimization Decision Tree
Research and Application Progress of Plasma Heating Technology for Continuous Casting Tundish

Related Author

Zhu Xida
Lu Jiasheng
Zhao Yongzhi
Liu Yu
Li Peng
Fang Yong
Ju Yulin
Cheng Xiaonong

Related Institution

Jiangyin China Resources Steelmaking Co., Ltd., Jiangyin
Zhejiang Institute of Advanced Materials, SHU
Jiangyin Xingcheng Special Steel Co.Ltd., Jiangyin
Jingkou Heat Treatment Service Station
School of Materials Science and Engineering, Jiangsu University
0