Effect of Cooling Rate on Mechanical Properties and Microstructure of New C61 Gear Steel
更新时间:2026-01-21
    • Effect of Cooling Rate on Mechanical Properties and Microstructure of New C61 Gear Steel

    • Special Steel   Vol. 44, Issue 2, Pages: 80-83(2023)
    • DOI:10.20057/j.1003-8620.2022-00106    

      CLC:
    • Received:26 September 2022,

      Online First:27 March 2023,

      Published:27 March 2023

    移动端阅览

  • 齐明, 梁晓东, 韩大虹, et al. Effect of Cooling Rate on Mechanical Properties and Microstructure of New C61 Gear Steel[J]. Special Steel, 2023, 44(2): 80-83. DOI: 10.20057/j.1003-8620.2022-00106.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Solution Heat Treatment Temperature and Cooling Mode on Microstructure and Mechanical Property of Ni-Cr-Mo-Co Alloy
Effect of Precipitate Phase Pretreatment on Microstructure and Mechanical Properties of High-strength Bolts
Dynamic CCT Curve and Microstructures of Antimony Micro-alloyed HRB500 Low-temperature Steel
Effect of C and Mo Content on Microstructure and Short-term Properties of IN617 Heat-resistant Alloy
The Post-forging Heat Treatment Process of 9Cr Martensitic Heat-resistant Steel

Related Author

Nie Yihong
Yang Xiaoyu
Wang Dapeng
Bai Xinghong
Peng Yamin
Bai Yaguan
Fu Wangtang
Wang Xu

Related Institution

China First Heavy Industries
Tianjin Heavy Industries Research & Development Co., Ltd.
State Key Laboratory of Metastable Material Science and Technology, Yanshan University
Special Steel Division, Nanjing Iron & Steel Co., Ltd.
Anhui university of Technology
0