Temperature Prediction of GCr15 Biilet Core Based on Heating Furnace Embedded Thermocouple Experiment
更新时间:2026-01-21
    • Temperature Prediction of GCr15 Biilet Core Based on Heating Furnace Embedded Thermocouple Experiment

    • Special Steel   Vol. 44, Issue 2, Pages: 1-6(2023)
    • DOI:10.20057/j.1003-8620.2022-00126    

      CLC:
    • Received:29 October 2022,

      Online First:22 March 2023,

      Published:22 March 2023

    移动端阅览

  • 韩怀宾, 虞学庆, 白瑞娟, et al. Temperature Prediction of GCr15 Biilet Core Based on Heating Furnace Embedded Thermocouple Experiment[J]. Special Steel, 2023, 44(2): 1-6. DOI: 10.20057/j.1003-8620.2022-00126.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

1

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Prediction of Remaining Molten Steel Volume during the Process of Ladle Slag Carry-over Based on SMOGN-XGBoost
Predictive Model for End Aim Temperature of Arc Furnace Based on Hybrid Genetic Algorithm

Related Author

Li Yahui
Zhao Deli
Wu Xiaolin
Yin Qing
Zhang Lifeng
Ren Ying
Xie Zhongyan
Duan Haojian

Related Institution

School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing
School of Mechanical and Materials Engineering, North China University of Technology
Jiangyin Xingcheng Special Steel Co., Ltd., Jiangyin
China First Heavy Machinery Corporation, Qiqihaer
北京科技大学信息工程学院
0