Inner-surface Cracks Analysis and Process Optimization of P92 Seamless Steel Pipe
During the production of large-sized P92 ferrite heat-resistant seamless steel pipe by rotary piercing process
the inner surface of the steel pipe is prone to produce small cracks. Through metallographic analysis
high-temperature phase transformation calculation and high-temperature heating test
the studies show that because of the higher heating temperature and the longer heating time
which increases the surface oxidation and decarburization
during the heating process of the P92 billet with a through hole in the center make a large number of high temperature δ ferrite phases near the inner wall and then the cracks generate and propagate around the δ Ferrite phases at the subsequent process of rotary piercing. According to the mechanism of in
ternal surface cracks
through the control of the Cr<13%
Ni
eq
<4% for P92 pipe chemical composition
the lowering of the billet heating temperature from 1220-1250 ℃ to 1190-1220℃
and the improvement parameters of roll speed
roll distance and the piercing point
the problem of cracks on the internal surface of large-diameter P92 seamless steel pipe is effectively solved
and the yield and production efficiency of P92 seamless steel pipe are improved.